Structure of Reversible Electrode Shelf Plasma cleaning improves wire-bonding, adhesion of resin molding, and wettability of underfill in the assembly process of semiconductor circuits, such as BGA, CSP, lead frames.and process assembly and other semiconductor lead frame.
The reversible electrode shelf can meet your various requirements. By reversing the shelf, you can convert RF electrode shelf to ground electrode and vise versa.



PC-300 Plasma Cleaner, PC-300 is equipped with the Reversible Electrode Shelves and enables easy switch of the plasma mode.
Additionally, PC-300 is simple, low-cost, and high-reliability system.