Celluloid Microenclosure and Microlens Array Fabricated by Suzukiʼs Universal Microprinting Method and XeF2 Vapor Etching for Microbial Analysis

Akihiro Matsutani1 and Ayako Takada2
1 Semiconductor and MEMS Processing Division, Technical Department, Tokyo Institute of Technology,
4259 Nagatsuta, Yokohama, Kanagawa 226-8503, Japan
2 Biomaterials Analysis Division, Technical Department, Tokyo Institute of Technology,
4259 Nagatsuta, Yokohama, Kanagawa 226-8501, Japan
Sensors and Materials, Vol. 30, No. 1 (2018) 149–155

A celluloid-based biochip for cell trapping is fabricated using Suzuki’s universal microprinting (SUMP) method. Samco tabletop Reactive Ion Etching (RIE) system was used for mold fabrication. Si layer was etched over photoresist and Cr mask in fluorine chemistry.