SAMCO UV-Ozone Cleaners are used for surface cleaning of substrates in device fabrication. This is testimonial from optoelectronics company in Fremont, CA.
The SAMCO UV-1 is a very simple-to-use system and can be effectively integrated into a controlled environment. The system’s internal cavity is leak tight at atmospheric conditions. The system is ideal for accomplishing two goals. First of all, it does an excellent job for treating bond surfaces. Our epoxy spreads about 30% more after the treatment. Secondly, the system is ideal for baking out moisture in the salts we use.