Scientific paper on organic FET fabrication from Carleton University

February 28, 2022 Samco 2022 Customer, Microfluidics, PMMA, Samco Customer Publication, Surface Treatment, UV-Ozone

A Low Temperature Processed, Soft-fluidic OEGFET Saliva Aptasensor for Cortisol

Roslyn S. Massey and Ravi Prakash
Department of Electronics Engineering, Carleton University, Ottawa, ON K1S 5B6, Canada;
IEEE Journal on Flexible Electronics, 1 – 1, 2022

Samco UV-Ozone cleaner UV-1 was used for PMMA surface treatment in biosensor fabrication.