Top-Down Nanofabrication and Characterization of 20 nm Silicon Nanowires for Biosensing Applications

M. Nuzaihan M. N 1, U. Hashim1,2, M. K. Md Arshad1,2, A. Rahim Ruslinda1, S.F.A. Rahman3, M. F. M. Fathil1, Mohd. H. Ismail2
1 Institute of Nano Electronic Engineering, Universiti Malaysia Perlis, 01000 Kangar, Perlis, Malaysia,
2 School of Microelectronic Engineering, Universiti Malaysia Perlis (UniMAP), 02600 Pauh, Perlis, Malaysia,
3 Chemistry Department, Faculty of Science, Universiti Putra Malaysia, 43400 UPM Serdang, Selangor, Malaysia
PLoS ONE 11(3): e0152318. doi:10.1371/journal.pone.0152318

Samco ICP etch system at Universiti Malaysia Perlis was used for anisotropic etching of silicon for silicon nanowires fabrication.