Unexpected Effects of the Rate of Deposition on the Mode of Growth and Morphology of Thin Films of Tetracene Grown on SiO2

R. K. Nahm and J. R. Engstrom
School of Chemical and Biomolecular Engineering, Cornell University, Ithaca, New York 14853, United States
J. Phys. Chem. C, 2016, 120 (13), pp 7183–7191
DOI: 10.1021/acs.jpcc.6b00963

Samco UV-Ozone cleaner at Cornell University was used for sample preparation before tetracene growth.