Scientific Paper on Nanowire Solar Cell by Kyung Hee University Team

January 16, 2015 Samco 2015 Customer, Samco Customer Publication, SU-8, Surface Treatment, UV-Ozone

Doubling Absorption in Nanowire Solar Cells with Dielectric Shell Optical Antennas

Sun-Kyung Kim Xing Zhang David J. Hill Kyung-Deok Song§ Jin-Sung Park§ Hong-Gyu Park§ and James F. Cahoon
Department of Applied Physics, Kyung Hee University, Gyeonggi-do 446-701, Republic of Korea
Department of Chemistry, University of North Carolina at Chapel Hill, Chapel Hill, North Carolina 27599-3290, United States
§Department of Physics, Korea University, Seoul 136-701, Republic of Korea
Nano Lett. 2015, 15, 753−758

Samco UV-Ozone cleaner, UV-1 was used for SU-8 stripping in nanowire-based device fabrication.