Scientific Paper on Nanoparticle Fabrication Using SAMCO UV-Ozone System from The City College of New York

January 7, 2016 Samco 2016 Customer, ITO, SAMCO Customer Publication, Surface Treatment, UV-Ozone

Electrostatically assisted fabrication of silver–dielectric core/shell nanoparticles thin film capacitor with uniform metal nanoparticle distribution and controlled spacing

Xue Lia, b, Olivia Niitsooa and Alexander Couzisa
a Department of Chemical Engineering, The City College of New York, NY 10031, United States
b Department of Chemical and Biomolecular Engineering, Lehigh University, Bethelehem, PA 18015, United States
Journal of Colloid and Interface Science (2016) 465, 333–341

Samco UV-Ozone cleaner at the City College of New York was used for UV-Ozone surface cleaning of ITO substrates before nanoparticle deposition.