Transparent Electrode Materials for Simultaneous Amperometric Detection of Exocytosis and Fluorescence Microscopy

Kassandra Kisler1, Brian N. Kim1, Xin Liu2, Khajak Berberian1, Qinghua Fang1, Cherian J. Mathai3, Shubhra Gangopadhyay3, Kevin D. Gillis2,4, and Manfred Lindau1
1 School of Applied and Engineering Physics, Cornell University, Ithaca, NY USA
2 Dalton Cardiovascular Research Center, University of Missouri, Columbia, MO USA
3 Department of Electrical and Computer Engineering, University of Missouri, Columbia, MO USA
4 Departments of Biological Engineering and Medical Pharmacology and Physiology, University of Missouri, Columbia, MO USA
J Biomater Nanobiotechnol. 2012 ; 3(2A): 243–253.

Samco UV-Ozone cleaner at Cornell University was used for photoresist descum in sample preparation.

Our UV-Ozone cleaners are equipped with stage heating and ozone generator, and they enable high-speed photoresist ashing & stripping. The processes can be applied for photoresist decsum application. For more information on our UV-Ozone cleaners, please visit the product page below.