Difference in growth and coalescing patterns of droplets on bi-philic surfaces with varying spatial distribution

Martand Mayukh Garimella, Sudheer Koppu, Shantanu Shrikant Kadlaskar, Venkata Pillutla, Abhijeet, Wonjae Choi
Department of Mechanical Engineering, University of Texas at Dallas, 800 W. Campbell Road, Richardson, TX 75080

Journal of Colloid and Interface Science (2017)

In this paper, surface wettability patterning was performed, and unique water droplet motion on the patterned regions was investigated. Samco UV-ozone cleaner, UV-1 at UT Dallas was used for complete native oxide removal after hydrofluoric acid treatment.

Surface wettability modulation (hydrophilic and hydrophobic) is fundamental for material research and device fabrication. Samco is developing surface treatment processes using UV-ozone technologies and plasma technologies. If you are interested in our latest material processing technologies and publication, please visit the page below.