Scientific Paper on AlN Nanocavity Fabrication Using AlN Plasma Etching from the University of Tokyo

High-Q AlN photonic crystal nanobeam cavities fabricated by layer transfer

S. Sergent1, M. Arita1, S. Kako1, K. Tanabe1, S. Iwamoto1,2 and Y. Arakawa1,2
1 Institute for Nano Quantum Information Electronics, The University of Tokyo, 4-6-1 Komaba, Meguro, Tokyo 153-8505, Japan
2 Institute of Industrial Science, The University of Tokyo, 4-6-1 Komaba, Meguro, Tokyo 153-8505, Japan
Appl. Phys. Lett. 101, 101106 (2012)

AlN nanopattern was fabricated by AlN plasma etching using Samco ICP etch system to improve the quality factor of nanobeam cavities.