Lateral distributed-feedback gratings for single-mode, high-power terahertz quantum-cascade lasers
M. Wienold, A. Tahraoui, L. Schrottke, R. Sharma, X. Lü, K. Biermann, R. Hey, and H. T. Grahn
Paul-Drude-Institut für Festkörperelektronik, Hausvogteiplatz 5-7, 10117 Berlin, Germany
Optics Express Vol.20, Issue 10, pp. 11207-11217 (2012)
SAMCO ICP Etching System was used for GaAs/AlGaAs dry etching over SiO2 mask in fabrication of Terahertz quantum-cascade lasers (THz QCLs).
For our capabilities of GaAs dry etching, please visit the process data page below.
GaAs Dry Etching Process (ICP-RIE)