Photonic Crystal Point-Shift Nanolasers With and Without Nanoslots—Design, Fabrication, Lasing, and Sensing Characteristics
Shota Kita, Kengo Nozaki, Shoji Hachuda, Hideki Watanabe, Yuji Saito, Shota Otsuka, Takeharu Nakada, Yoshiki Arita, and Toshihiko Baba
Department of Electrical and Computer Engineering, Yokohama National University, 79-5 Tokiwadai, Hodogaya-ku, Yokohama 240-8501, Japan
IEEE Journal of Selected Topics in Quantum Electronics, (2011) 17, 6
SAMCO ICP Etch System was used for recipe optimization of InP plasma etching. InP etch profile with a high aspect-ratio was successfully fabricated.
For our process capabilities of InP plasma etching, please visit the page below.
InP Dry Etching Process (RIE or ICP-RIE)