Basic Plasma Research Kit

SAMCO’s Basic Plasma Research Kit (BP-1) is designed for diverse thin-film experiments using plasma chemical reactions. This system serves as an ideal educational tool, offering an introduction to the fundamental basics of plasma physics.

The system features a reaction chamber with parallel plate electrode that can process samples up to 100 mm. The electrode spacing can be manually adjusted from 10-40 mm.

The BP-1 has been used for plasma polymerization, surface modification, dry etching and thin film deposition. However as this is a fully manual system with minimal safety mechanisms, it is usually recommended for advanced users that would otherwise consider a “home-built” plasma system, or for kinetic studies of the plasma process using inert gases.

We highly recommend that prospective purchasers also consider more advanced systems for etching or deposition.

The standard system includes:

  • Manual throttle valve for pressure control
  • 2 rotameters for gases
  • 200 W RF generator and manual matching network
  • Mineral based rotary pump

Options include stage heating up to 400°C.