Positive onset potential and stability of Cu2O-based photocathodes in water splitting by atomic layer deposition of a Ga2O3 buffer layer
Changli Lia, Takashi Hisatomib, Osamu Watanabeb, Mamiko Nakabayashic, Naoya Shibatac, Kazunari Domenb and Jean-Jacques Delaunaya
Energy Environ. Sci., 2015, 8, 1493
Photoelectrochemical (PEC) water splitting system is a promising application for H2 production as next-generation clean energy. To achieve stable and efficient water splitting reaction of Cu2O-based photocathodes, Ga2O3 film was introduced as a buffer layer between the Cu2O layer and the TiO2 protective layer. Samco Plasma Etching System (RIE etcher) at the University of Tokyo was used for argon plasma treatment of Cu2O layer to remove the residual contaminants from the annealing and change the hydrophobic surface to a hydrophilic surface.
Samco offers plasma cleaners as well as RIE etchers for plasma surface treatment of various samples. Please visit the product pages below for more details of our plasma cleaners.
General Plasma Cleaners
Remote Plasma Cleaners (Downstream Plasma)