Multi-channel PMMA microfluidic biosensor with integrated IDUAs for electrochemical detection
Nongnoot Wongkaewa,b, Peng Heb, Vanessa Kurthb, Werasak Surareungchaia, and Antje J. Baeumnerb
aSchool of Bioresources and Technology, King Mongkut’s University of Technology Thonburi, Bangkhuntien, Bangkok 10150,Thailand bDepartment of Biological and Environmental Engineering, Cornell University, 202 Riley Robb Hall, Ithaca, NY 14853, USA
Anal Bioanal Chem. 2013 July ; 405(18): 5965–5974. doi:10.1007/s00216-013-7020-0.
Samco UV-Ozone Cleaner at Cornell University was used for oxidation of PMMA to generate carboxylic groups on the surface in microfluidic biosensor fabrication. Samco UV-Ozone cleaners are used for many R&D labs of polymer biosensor fabrication for bonding of polymer materials, such as PDMS, PMMA , COP & COC.