Enhancement-mode hydrogenated diamond metal-oxide-semiconductor field-effect transistors with Y2O3 oxide insulator grown by electron beam evaporator
J. W. Liu1 H. Oosato2 M. Y. Liao1 and Y. Koide3
1 Research Center for Functional Materials, National Institute for Materials Science (NIMS), 1-1 Namiki,
Tsukuba, Ibaraki 305-0044, Japan
2 Nanofabrication Platform, NIMS, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047, Japan
3 Research Network and Facility Services Division, NIMS, 1-2-1 Sengen, Tsukuba, Ibaraki 305-0047, Japan
APPLIED PHYSICS LETTERS 110, 203502 (2017)
Hydrogenated diamond-based MOSFET is a promising next-generation power device as well as SiC- or GaN-based devices. The device research on this material is still under development.
In this paper, H-diamond MOSFET with an Y2O3 oxide insulator was fabricated. Samco RIE etcher, RIE-200NL was used for mesa etching of H-diamond layer.
Samco RIE etchers offer diamond plasma etching process solutions for emerging power device research communities. For more details on our equipment lineup and specifications, please visit the product page below.
RIE Etcher for R&D and Production
If you are interested in diamond etching processes, please visit the process data page below.
Diamond Plasma Etching