Scientific Paper on InP Microenclosure Array Fabrication Using InP Plasma Etching from Tokyo Institute of Technology

Single-Cell Isolation and Size Sieving Using Microenclosure Array for Microbial Analysis

Akihiro Matsutani* and Ayako Takada1
Semiconductor and MEMS Processing Center, Tokyo Institute of Technology, 4259 Nagatsuta, Midori-ku, Yokohama 226-8503, Japan
1Biomaterial Analysis Center, Tokyo Institute of Technology, 4259 Nagatsuta, Midori-ku, Yokohama 226-8501, Japan
Sensors and Materials, Volume 27, Number 5 (2015)

Samco open-load ICP etch system was used for fabrication of micropillar fabrication on InP substrates for cell isolation and size sieving.


For more details of our InP plasma etching capabilities, please visit the page below.
InP Dry Etching Process (RIE or ICP-RIE)