Scientific Paper on UV LED fabrication from National Cheng Kung University, Taiwan

Improving the Brightness and Reliability of InGaN/GaN Near Ultraviolet Light Emitting Diodes by Controlling the Morphology of the GaN Buffer Layer

S. C. Tsai, H. C. Fang, C. H. Lu and Y. L. Lai
National Cheng Kung University, Tainan, Taiwan
Journal of Display Technology (2016) (Volume:PP , Issue: 99 )

Samco ICP etch system at National Cheng Kung University was used for InGaN/GaN dry etching in UV LED fabrication.