Constrained spheroids for prolonged hepatocyte culture
Wen Hao Tonga, b, c, Yu Fanga, b, c, Jie Yana, c, g, Xin Hongc, Nisha Hari Singha,
Shu Rui Wangd, Bramasta Nugrahaa, b, e, f, Lei Xia c, Eliza Li Shan Fongc,
Ciprian Iliescua, Hanry Yua, b, c, g, h, i,
a Institute of Biotechnology and Nanotechnology, A*STAR, The Nanos, #04-01, 31 Biopolis Way, Singapore 138669, Singapore
b NUS Graduate School for Integrative Sciences and Engineering, Centre for Life Sciences (CeLS), #05-01, 28 Medical Drive, Singapore 117456, Singapore
c Department of Physiology, Yong Loo Lin School of Medicine, MD9-03-03, 2 Medical Drive, Singapore 117597, Singapore
d Bruker Singapore Pte Ltd., 11 Biopolis Way #10-10, The Helios, Singapore 138667, Singapore
e ETH Zürich, Department of Biosystem Science and Engineering (D-BSSE), Mattenstrasse 26, CH-4058 Basel, Switzerland
f Roche Pharmaceutical Research and Early Development, Department of Discovery Technology, Roche Innovation Center Basel, Grenzacherstrasse 124,
CH-4070 Basel, Switzerland
g Singapore-MIT Alliance for Research and Technology, 1 CREATE Way, #10-01 CREATE Tower, Singapore 138602, Singapore
h Mechanobiology Institute, National University of Singapore, T-Lab, #05-01, 5A Engineering Drive 1, Singapore 117411, Singapore
i Department of Biological Engineering, Massachusetts Institute of Technology, Cambridge, MA 02139, USA
Biomaterials (2016) 80 106e120
Samco Basic Plasma Kit was used for surface oxidation of Parylene C membrane in O2 plasma in sample preparation.