Fabrication of SiNx Thin Film of Micro Dielectric Barrier Discharge Reactor for Maskless Nanoscale Etching
Qiang Li1, Jie Liu1, Yichuan Dai1, Wushu Xiang1, Man Zhang1, Hai Wang2 and Li Wen1
1 Department of Precision Machinery and Precision Instrumentation, University of Science and Technology of China, Hefei 230027, China
2 School of Mechanical and Automotive Engineering, Anhui Polytechnic University, Wuhu 241000, China
Micro dielectric barrier discharge (MDBD) devices have some potential interesting applications such as surface modification. Silicon Nitride (SiNx) film can be used as a dielectric barrier layer material in MDBD devices. However, there are challenges of crack and wrinkle formation due to mechanical stress of SiNx film in device fabrication. Samco plasma CVD system was used for SiNx film deposition. With optimization of deposition process recipe, compressive stress of SiNx film was mitigated to suppress crack formation.
For more details of our SiNx film deposition capabilities, please visit the process data page below.
SiNx PECVD Process