Precise etching control
Square-shaped pillars with a width of 28 μm were successfully fabricated using the Bosch Process. The pillars maintain their square geometry from top to bottom, demonstrating precise etching control.
- Pillar height: 450 μm
- Profile angle: 89.9°
Photo courtesy of National Taiwan University.