Scientific Paper on Boron-doped DLC Film Deposition from Yamaguchi University
Enhancement of electrical conductivity and electrochemical activity of hydrogenated amorphous carbon by incorporating boron atoms
Hiroshi Naragino, Kohsuke Yoshinaga, Akira Nakahara, Sakuya Tanaka and Kensuke Honda
Graduate school of Science and Engineering, Yamaguchi University, 1677-1, Yoshida, Yamaguchi-shi, Yamaguchi 753-8512, Japan
Journal of Physics: Conference Series, 441, 2013 conference 1
Process and film properties of conductive boron-doped hydrogenated amorphous carbon (B-DLC) thin films was studied in this research. Samco PECVD system at Yamaguchi University was used for DLC film deposition.
Samco offers PECVD systems and process technology for deposition of various types of films such as SiO2, SiNx, TiO2, amorphous carbon (a-Si), SiON, SiCN and DLC.
For more details of our system lineup, please visit the product pages below.
Anode PECVD Systems for High-quality Film Deposition
Cathode PECVD Systems for High-speed SiO2 and SiNx Film Deposition under 80 °C