Category: FeSi2 Etch
Scientific Paper on FeSi2 Plasma Etching from University of Tsukuba
Reactive Ion Etching of β-FeSi2 with Inductively Coupled Plasma
Takayuki Wakayama, Takashi Suemasu, Tomomi Kanazawa and Hiroyuki Akinaga
Institute of Applied Physics, University of Tsukuba, Tsukuba, Ibaraki 305-8573, Japan
Jpn. J. Appl. Phys. (2006) 45 L569
Samco ICP-RIE etcher was used for plasma etch recipe development of β-FeSi2 on a silicon substrate using fluorine chemistry.
High etch selectivity of β-FeSi2 against silicon was investigated.
Please visit our product page for more details of our ICP plasma etch systems.
ICP Plasma Etch Systems for Si, SiO2, III-V & Metal