Category: PMMA Etch

01 Mar

Scientific Paper on Gold Nanoslit Fabrication Using PMMA Etching from Fudan University Team

Samco 2017 Customer, Other Materials Etch, PMMA Etch, Samco Customer Publication

A novel PMMA/NEB bilayer process for sub-20 nm gold nanoslits by a selective electron beam lithography and dry etch

Xiaqi Huanga, Jinhai Shaoa, ChialinTsoua, Sichao Zhanga, Bingrui Lua, Ling Haob, Yan Sunc, and Yifang Chena
a Nanolithogrophy and Application Research Group, State Key Lab of ASIC and System, School of Information Science and Engineering, Fudan University, Shanghai 200433, China
b National Physical Laboratory, Teddington TW11 0LW, UK
c National Laboratory for Infrared Physics, Shanghai Institute of Technical Physics, Chinese Academy of Sciences, Shanghai, China
Microelectronic Engineering (2017) 172, Pages 13-18

Gold nanoslit structures were fabricated using process parameter optimization of electron beam lithography and dry etching. Samco plasma etcher RIE-10NR was used for dry etching of PMMA layer in oxygen plasma treatment.

11 Nov

Scientific Paper on Wrinkled PDMS Film Fabrication from Nanjing University, China

Samco 2012 Customer, Other Materials Etch, PMMA Etch, Resist, Samco Customer Publication

Crack-free controlled wrinkling of a bilayer film with a gradient interface

Yan Xuana Xu Guoa Yushuang Cuia Changsheng Yuana Haixiong Gea Bo Cuib and Yanfeng Chena
National Laboratory of Solid State Microstructures, Department of Materials Science and Engineering, College of Engineering and Applied Sciences, Nanjing University, Nanjing, 210093, China
Department of Electrical and Computer Engineering, University of Waterloo, 200 University Avenue, West Waterloo, Ontario N2L3G1, Canada
Soft Matter (2012) 8, 9603

SAMCO Plasma Etching System (RIE etcher) was used for plasma etching of silicon-containing resist and PMMA to fabricate wrinkled films.