High-precision Si microfluidic channel etching

Microfluidic channels with a width of 3 μm were fabricated using the Bosch process on the RIE-400iPB system. This vertical deep etching method ensures precise control over channel geometry, making it ideal for lab-on-a-chip applications and biomedical research.

 