Scientific Paper on ZnO Nanorods Functionalization from Linköping University, Sweden

February 19, 2014 Samco 2014 Customer, Plasma Treatment, Samco Customer Publication, Surface Treatment, ZnO

The improved piezoelectric properties of ZnO nanorods with oxygen plasma treatment on the single layer graphene coated polymer substrate

Mushtaque Hussain, Mazhar Ali Abbasi, Zafar Hussain Ibupoto, Omer Nur and Magnus Willander
Physical Electronic & Nanotechnology division, Department of Science &Technology, Campus Norrköping, Linköping University, SE-60174 Norrköping, Sweden.
physica status solidi (a) Volume 211, Issue 2, pages 455–459, February 2014

ZnO Periodic Table

ZnO nanorods were treated with an oxygen plasma using SAMCO RIE Plasma Etching System to reduce the defect levels.